The quality of Austempered Ductile Iron, ADI, made from lndonesianproduced Ferro-Casting Ductile Iron, FCDI, as base material is discussed. FCDI that is made for routine consumption in Indonesia; not especially as ADl base material, is assessed for chemical composition and mechanical properties. It is then austempered at austenisation temperature 950°C with 1 hour holding. Three austempering temperatures, 300°C, 350°C, and 400°C, were investigated with 1 hour holding time using fluidized bed furnace. Metallographic examinations, tension tests and Brinen hardness number tests, were then carried out for the resulting ADI. Based on ASTM A897M - 90, the products of austempering temperature 300°C and 350°C can be classified as ADl 850/550/10. This shows that the Indonesian-produced FCDI base material can be used for ADI production.
Bagikan artikel ini di:
Situs web ini menggunakan cookie untuk meningkatkan pengalaman Anda menggunakan situs web. Kami juga dapat menggunakan cookie untuk menganalisis data situs web sehingga kami dapat meningkatkan layanan online kami. Untuk mengetahui lebih lanjut, kunjungi kebijakan privasi.